This paper presents the measurements of the air flow resistance of polyamide 12 samples
made by selective laser sintering. The results have shown that, due to the porosity of the
microstructure, the samples with thickness smaller than 1.7 mm cannot be considered airtight,
while the samples with thickness 2.2 mm are airtight. The airflow resistance of the samples that
allow airflow increases with air speed.